• Prevents corrosion under insulation of carbon steel. Resistant
to boiling water and 1200°F (648.8°C). Direct application to ambient and hot steel 50°F to
500°F (10°C to 260°C).
• Prevents chloride induced external stress cracking of insulated stainless
steel. Resistant to boiling water and 1200°F (648.8°C). Direct application to ambient and hot
steel 50°F to 500°F (10°C to 260°C).
• High build primer, direct application to ambient and
hot steel 50°F to 500°F (10°C to 260°C) resistant to 1200°F (648.8°C). Topcoat with Hi-Temp
colors.
• Apply direct to rust. High build and heat resistant to 1000°F (537.7°C). Direct application
to ambient and hot steel 50°F to 500°F (10°C to 260°C). Use on both insulated and un-insulated
topcoats with Hi-Temp colors.
• Protects cryogenic equipment; withstands severe cold to hot thermal
cycling; resistance of -300°F to 1000°F (-184°C to 537.7°C).